1. In the normal production process, potassium chloride, boric acid and zinc chloride are analyzed and adjusted once a week.
2. HL-93 brightener should be added according to the consumption of 60-80 ml per KA. h. When adding, it is necessary to dilute 2-3 times with plating solution.